Skip to main content

Table 1 Diameters of the ZnO/CAT and ZnO/CA microparticles

From: In vitro physiological and antibacterial characterization of ZnO nanoparticle composites in simulated porcine gastric and enteric fluids

Sample

d10% (μm)

d50% (μm)

d90% (μm)

d4,3 (μm)

Span (μm)

ZnO/CAT

18.59

109.63

216.46

114.32

1.80

ZnO/CA

47.92

169.11

257.16

162.48

1.24